Long epoxy session

Have tacked and taped the seams during a big four hour epoxy session. The internal seams have been filleted apart from where the angle was too flat and so glass tapped with 50mm tape. Also tacked externally the top seam and around the bow area. The fillets easily created with tongue depressor and the cleaned up with a wood chisel made from the tongue depressor. The glass tape was prepared on a glassing table and finished with peel ply. Now nicely cooking at twenty degrees.

Built time total 25 hours

Epoxy total 366ml